NS-EN ISO 2566-1:1999

NOK 828,00 (excl. VAT) InformationMonitor standard
basket Webprint basket Printed and bound
Get online access
Status: Alert Withdrawn
Norwegian title: Stål — Omregning av forlengelsesverdier — Del 1: Karbon- og lavlegerte stål (ISO 2566-1:1984)
English title: Steel — Conversion of elongation values — Part 1: Carbon and low alloy steels (ISO 2566-1:1984)
Item type: Standard
Language: Engelsk
Edition: 1 (1999-11-10)
Superseded by: NS-EN ISO 2566-1:2021 Check Published
Number of pages: 36
Price:

NOK 828,00 (excl. VAT)
NOK 1 035,00 (with VAT)

Included in: NS ICS 77.040
NS ICS 77.040.10
NS ICS 77
Scope: This part of IS0 2566 specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths. The formula (see clause 4) on which conversions are based is considered to be reliable when applied to carbon, carbon manganese, molybdenum and chromium molybdenum steels within the tensile strength range 300 to 700 N/mm2 and in the hot-rolled, hot-rolled and normalized or annealed conditions, with or without tempering. These conversions are not applicable to a) cold reduced steels; b) quenched and tempered steels; c) austenitic steels. Neither should they be used where the gauge length exceeds 25 VSo or where the width to thickness ratio of the test piece exceeds 20. Care should be exercised in the case of strip under 4 med mer thickness, as the index in the formula given in clause 4 increases with decreasing thickness; the value to be used shall be the subject of agreement between the customer and the supplier.
Adopted: 1999-11-10
Withdrawn: 2022-01-07
ICS: 77.040.10 - Mekanisk prøving av metaller